Room-temperature coercivity enhancement in mechanically alloyed antiferromagnetic-ferromagnetic powders

Autor/a

Sort Viñas, Jordi

Nogués, Josep

Amils Capdevila, Xavier

Suriñach, Santiago

Muñoz Domínguez, Juan Santiago

Baró, M. D.

Data de publicació

1999

Resum

This article may be downloaded for personal use only. Any other use requires prior permission of the author and the American Institute of Physics.


The coercivity,HC, and squareness of Co powders have been enhanced at room temperature by mechanically alloying them with antiferromagneticpowders with Néel temperature, TN, above room temperature. The enhancement is maximum after field annealing above TN. The existence of loop shifts and the dependence of HC on the annealing and measuring temperatures indicate that exchange bias effects are responsible for this behavior.

Tipus de document

Article

Llengua

Anglès

Matèries i paraules clau

Powders; Annealing; Antiferromagnetism; Coercive force; Alloys; Exchange interactions; Temperature measurement

Publicat per

 

Documents relacionats

Applied physics letters ; Vol. 75, Issue 20 (November 1999), p. 3177-3179

Drets

open access

Aquest material està protegit per drets d'autor i/o drets afins. Podeu utilitzar aquest material en funció del que permet la legislació de drets d'autor i drets afins d'aplicació al vostre cas. Per a d'altres usos heu d'obtenir permís del(s) titular(s) de drets.

https://rightsstatements.org/vocab/InC/1.0/

Aquest element apareix en la col·lecció o col·leccions següent(s)