Room-temperature coercivity enhancement in mechanically alloyed antiferromagnetic-ferromagnetic powders

Autor/a

Sort Viñas, Jordi

Nogués, Josep

Amils Capdevila, Xavier

Suriñach, Santiago

Muñoz Domínguez, Juan Santiago

Baró, M. D.

Fecha de publicación

1999

Resumen

This article may be downloaded for personal use only. Any other use requires prior permission of the author and the American Institute of Physics.


The coercivity,HC, and squareness of Co powders have been enhanced at room temperature by mechanically alloying them with antiferromagneticpowders with Néel temperature, TN, above room temperature. The enhancement is maximum after field annealing above TN. The existence of loop shifts and the dependence of HC on the annealing and measuring temperatures indicate that exchange bias effects are responsible for this behavior.

Tipo de documento

Article

Lengua

Inglés

Materias y palabras clave

Powders; Annealing; Antiferromagnetism; Coercive force; Alloys; Exchange interactions; Temperature measurement

Publicado por

 

Documentos relacionados

Applied physics letters ; Vol. 75, Issue 20 (November 1999), p. 3177-3179

Derechos

open access

Aquest material està protegit per drets d'autor i/o drets afins. Podeu utilitzar aquest material en funció del que permet la legislació de drets d'autor i drets afins d'aplicació al vostre cas. Per a d'altres usos heu d'obtenir permís del(s) titular(s) de drets.

https://rightsstatements.org/vocab/InC/1.0/

Este ítem aparece en la(s) siguiente(s) colección(ones)