Degradation of thin tungsten filaments at high temperature in HWCVD

Data de publicació

2015-01-27T09:24:59Z

2015-01-27T09:24:59Z

2015

2015-01-27T09:24:59Z

Resum

The degradation of the filaments is usually studied by checking the silicidation or carbonization status of the refractory metal used as catalysts, and their effects on the structural stability of the filaments. In this paper, it will be shown that the catalytic stability of a filament heated at high temperature is much shorter than its structural lifetime. The electrical resistance of a thin tungsten filament and the deposition rate of the deposited thin film have been monitored during the filament aging. It has been found that the deposition rate drops drastically once the quantity of dissolved silicon in the tungsten reaches the solubility limit and the silicides start precipitating. This manuscript concludes that the catalytic stability is only guaranteed for a short time and that for sufficiently thick filaments it does not depend on the filament radius.

Tipus de document

Article


Versió acceptada

Llengua

Anglès

Publicat per

Elsevier B.V.

Documents relacionats

Versió postprint del document publicat a: http://dx.doi.org/10.1016/j.tsf.2014.10.011

Thin Solid Films, 2015, vol. 575, p. 34-37

http://dx.doi.org/10.1016/j.tsf.2014.10.011

Citació recomanada

Aquesta citació s'ha generat automàticament.

Drets

(c) Elsevier B.V., 2015

Aquest element apareix en la col·lecció o col·leccions següent(s)