Degradation of thin tungsten filaments at high temperature in HWCVD

Fecha de publicación

2015-01-27T09:24:59Z

2015-01-27T09:24:59Z

2015

2015-01-27T09:24:59Z

Resumen

The degradation of the filaments is usually studied by checking the silicidation or carbonization status of the refractory metal used as catalysts, and their effects on the structural stability of the filaments. In this paper, it will be shown that the catalytic stability of a filament heated at high temperature is much shorter than its structural lifetime. The electrical resistance of a thin tungsten filament and the deposition rate of the deposited thin film have been monitored during the filament aging. It has been found that the deposition rate drops drastically once the quantity of dissolved silicon in the tungsten reaches the solubility limit and the silicides start precipitating. This manuscript concludes that the catalytic stability is only guaranteed for a short time and that for sufficiently thick filaments it does not depend on the filament radius.

Tipo de documento

Artículo


Versión aceptada

Lengua

Inglés

Publicado por

Elsevier B.V.

Documentos relacionados

Versió postprint del document publicat a: http://dx.doi.org/10.1016/j.tsf.2014.10.011

Thin Solid Films, 2015, vol. 575, p. 34-37

http://dx.doi.org/10.1016/j.tsf.2014.10.011

Citación recomendada

Esta citación se ha generado automáticamente.

Derechos

(c) Elsevier B.V., 2015

Este ítem aparece en la(s) siguiente(s) colección(ones)